Materials

Identification of material model of TiN using numerical simulation of nanoindentation test

Contributing authors of JOANNEUM RESEARCH:
Authors
M. Kopernik, R. Major, A. Milenin; Lackner, J. M.
Title:
Identification of material model of TiN using numerical simulation of nanoindentation test
Seiten:
604-616